ny_banner

umkhiqizo

I-Multifunctional Alkyd Anti Rust Primer Paint For Metal Protection

Incazelo emfushane:

Yakhiwe nge-alkyd resin eguquliwe, i-antirust pigment, i-extender pigment, i-drier, i-organic solvent, njll. I-Alkyd iron red antirust primer yenziwa ngokungeza impushana ebomvu ebomvu, i-extender pigment, i-solvent kanye ne-axiliary.


IMINININGWANE EYEngeziwe

*Ividiyo:

https://youtu.be/xHcfaxVdt8k?list=PLrvLaWwzbXbi5Ot9TgtFP17bX7kGZBBRX

*Izici Zomkhiqizo:

.Ukwakhiwa okulula, umbala ogqamile, okhanyayo futhi onzima;
.Ukumelana nokugqwala okuhle;
.Ukunamathela okuhle kwefilimu kapende, ukumelana nokugqwala okuphezulu;
.Ukumelana namanzi okuqinile, ukomisa ngokushesha ekamelweni lokushisa

*Uhlelo Lomkhiqizo:

Isetshenziselwa ikakhulukazi indawo yensimbi kanye ne-anti-rust coating, ikakhulukazi esetshenziselwa imishini yemishini, isakhiwo sensimbi, ipayipi, njll.
Upende obomvu we-Alkyd obomvu we-antirust ulungele ukuvimbela ukugqwala kwezindawo zensimbi ezisansimbi njengamabhuloho, imibhoshongo yensimbi, nokwakhiwa kwemishini yensimbi emikhulu yezimoto.Awukwazi ukusetshenziselwa amapuleti e-aluminium, amapuleti e-zinc, njll.

*Imininingwane yobuchwepheshe:

Into

Okujwayelekile

Umbala

I-ayoni ebomvu, empunga noma omunye umbala

Okuqukethwe okuqinile, %

≥39.5

ukuguquguquka, mm

≤3

Iphoyinti elikhanyayo, ℃

38

Ugqinsi lwefilimu elomile, um

30-50

Isikhathi sokumisa (25 degrees C), H

indawo yomile≤ 2h, yomile kanzima≤ 24h

Ukumelana namanzi kasawoti

Amahora angu-24, akukho bhamuza, akukho ukuwa, akukho ukushintsha kombala

Izinga Lereferensi:HG/T 2009-1991

*Indlela yokwakha:

1. Ukufutha komoya nokuxubha kwamukelekile.

2. I-substrate kufanele ihlanzwe ngaphambi kokusetshenziswa, ngaphandle kwamafutha, uthuli, ukugqwala, njll.

3. I-viscosity ingalungiswa nge-X-6 alkyd diluent.

4. Uma ufutha i-topcoat, uma i-gloss iphakeme kakhulu, kufanele iphuculwe ngokulinganayo nge-sandpaper ye-mesh engu-120 noma ngemva kokuba ubuso bejazi langaphambilini bomile futhi ukwakhiwa kwenziwa ngaphambi kokuba kumiswe.

5. I-alkyd anti-rust paint ayikwazi ukusetshenziswa ngokuqondile ku-zinc kanye ne-aluminium substrates, futhi inokumelana nesimo sezulu esibi uma isetshenziswa iyodwa, futhi kufanele isetshenziswe ngokuhambisana ne-topcoat.

*Ukwelashwa komhlaba:

Ingaphezulu le-primer kufanele lihlanzeke, lome futhi lingangcoli.Sicela unake isikhawu sokumboza phakathi kokwakhiwa kanye ne-primer.
Zonke izindawo kufanele zihlanzeke, zome futhi zingangcoli.Ngaphambi kokudweba, kufanele kuhlolwe futhi kuphathwe ngokuhambisana nezinga le-ISO8504:2000.

*Ukwelashwa komhlaba:

Ingaphezulu le-primer kufanele lihlanzeke, lome futhi lingangcoli.Sicela unake isikhawu sokumboza phakathi kokwakhiwa kanye ne-primer.

*Umbandela Wokwakha:

Izinga lokushisa lesisekelo alikho ngaphansi kuka-5 ℃, futhi okungenani 3 ℃ kunezinga lokushisa lendawo yamazolo, umswakama ohlobene kufanele ube ngaphansi kuka-85% (kufanele ulinganiswe eduze nesisekelo sezinto), inkungu, imvula, iqhwa, umoya. futhi imvula ivinjelwe ngokuphelele ukwakhiwa.

*Iphakheji:

Upende:20Kg/Ibhakede;4Kg/Ibhakede, 200Kg/ ibhakede